Interface Degradation of LaCl3-Based Solid Electrolytes Coupled with Ultrahigh-Nickel Cathodes.

Ye-Chao Wu,Feng Li,Xiaobin Cheng,Yihong Tan,Xin Huang,Jin-Da Luo,Shu Chen,Ruijun Pan,Yi-Chen Yin,Zheng Liang,Hong-Bin Yao
DOI: https://doi.org/10.1021/acs.nanolett.4c03502
IF: 10.8
2024-01-01
Nano Letters
Abstract:Despite competitive compatibility with high-nickel cathodes, chloride solid electrolytes (SEs) still experience inevitable side reactions at the cathode/SE interface, causing capacity decay in all-solid-state lithium batteries (ASSLBs) during cycling. Herein, a three-electrode ASSLB testing device is developed to comprehensively reveal the interface failure mechanisms of the ultrahigh-nickel LiNi0.92Co0.05Mn0.03O2 (NCM92) cathode paired with LaCl3-based chloride SE Li0.447La0.475Zr0.059Ta0.179Cl3 (LLZTC). Distribution of relaxation time (DRT) analysis clearly shows the ASSLB degradation accompanied by a significant NCM92/LLZTC interface impedance increase, which becomes more pronounced at the higher cutoff charging voltage of 4.8 V vs Li+/Li. Furthermore, time-of-flight secondary ion mass spectrometry (ToF-SIMS) and focused ion beam scanning electron microscopy (FIB-SEM) analysis also confirm the deterioration arising from active lattice oxygen and loss of physical contact at the NCM92/LLZTC interface. These findings reveal both electrochemical degradation and physical contact failure at the cathode/SE interface as key causes of the ASSLBs' capacity decay.
What problem does this paper attempt to address?