Abstract:In order to better understand the confinement effect of CNTs on the properties of Ni based catalysts, Ni/CNTs catalysts with different Ni locations via the modification of CNTs pretreatment and impregnation process were prepared, characterized and tested in glycerol steam reforming. The Ni-in/CNTs catalyst showed excellent low temperature reaction activity, with initial Ni time yield of 0.064 molC3H8O3 & sdot;gNi - 1 & sdot;h- 1 and H2 yield of 50.1% at 275 degrees C, 0.1Mpa. The confinement of Ni particles inside CNTs nanotubes led to more active sites with weak H2 absorption strength, which were more related to the activity for glycerol steam reforming reaction. All the catalysts exhibited a noticeable deactivation during the reaction, however, their main deactivation mechanisms were not the same. The confinement effect of CNTs nanotubes could limit the sintering degree of Ni particles, and thus the deactivation of Ni-in/CNTs catalyst was slow in the initial stage; nevertheless, its deactivation became faster in the subsequent stage, which was due to the severe carbon deposition. For the two catalysts with Ni particles on the outer surface of supports, their main deactivation reason was the significant sintering of Ni species, and therefore, their deactivation was faster first and then slow down.
What problem does this paper attempt to address?