Strategies of Reducing the Heat-Affected Zone in Mg/steel Resistance Riveting Welding Joints for Improving Joint Quality

Liangyu Fei,Fei Jiang,Peng Zhang,Chao Chen,Zhenhao Zheng,Jusen Li,Shengdun Zhao,Ninshu Ma
DOI: https://doi.org/10.1016/j.jmapro.2024.06.070
IF: 5.684
2024-01-01
Journal of Manufacturing Processes
Abstract:This study employs two methods, adding a zinc interlayer and increasing rivet length, to mitigate the heat- affected zone (HAZ) of Mg in Mg and steel resistance riviting welding (RRW) joints, aiming to enhance the mechanical properties of the joints. The initial optimal peak load for RRW joints was 4892N. For joints with a Zn interlayer, although the HAZ could be reduced, the excessive consumption of welding heat by Zn resulted in a less satisfactory tensile-shear peak load of 4615N. On the other hand, increasing the rivet length improved the mechanical performance of the joints. Specifically, using a longer rivet and a lower piercing current of 13kA, the average peak load of the joint was 5491N. When choosing a higher piercing current, the average peak load of the joint increased to 6079N. Further comparison of the microstructure of joints using long rivets revealed that at the same observation position in Mg's HAZ, the average grain size was 7.91 mu m with a higher piercing current and 15.12 mu m with a lower piercing current. It can be inferred that the HAZ of Mg is smaller at higher piercing currents. Hardness measurements of the joints supported this conclusion. Finally, a comparison of the failure modes of the joints was conducted. With the increase in welding current, the joint's failure mode transitioned from interface fracture to pull-out fracture, ultimately transforming into base material pull off fracture.
What problem does this paper attempt to address?