Microstructure and mechanical properties of resistance element welded joints for DP780 steel and 6061 aluminum alloy

Yue Yang,Yuanbo Bi,Yixuan Zhang,Jie Su,Zhen Luo
DOI: https://doi.org/10.1002/adem.202201795
IF: 3.6
2023-02-09
Advanced Engineering Materials
Abstract:DP780 steels and 6061‐T6 aluminum alloys were joined using the resistance element welding process with a flat Q235 rivet. The macrostructure, microstructure and mechanical properties of the REW joints were investigated. The nugget zone and upper heat‐affected zone microstructure of exhibited lath martensite. The inter‐critical heat‐affected zone microstructure of consisted of ferrite and martensite. The microstructure of Al nugget near the Q235 rivet consisted of columnar dendrites. Two types of intermetallic compound (IMC) layers were formed at the steel/Al interface. A tongue‐like Fe2Al5 layer was found adjacent to the steel side, while a needle‐like Fe4Al13 layer was found adjacent to the aluminum alloy side. The welding current has a significant influence on the nugget size, peak load and energy absorption of joints. The fracture behavior analysis of the REW joints was performed using the in‐situ digital image correlation (DIC) method. There are two failure modes of the REW joint under different welding currents: pull‐out failure (PF) and the base material pull‐out failure (BPF). At a welding current of 17 kA, the maximum tensile shear value of the REW joints was 6.27 kN with a nugget diameter of 5.37 mm. The failure mode of the REW joints was mainly BPF mode exhibited superior lap‐shear performance. This article is protected by copyright. All rights reserved.
materials science, multidisciplinary
What problem does this paper attempt to address?