Melting Properties and Phase Composition Transformation of Ti-Bearing Electric Furnace Slags in CaO–SiO 2 –MgO–Al 2 O 3 –50%TiO 2 System

Jianfa Jing,Yufeng Guo,Shuai Wang,Feng Chen,Lingzhi Yang,Jianfeng Yang,Fuchun Xu,Linxuan Yu
DOI: https://doi.org/10.1007/s12540-024-01630-y
IF: 3.451
2024-01-01
Metals and Materials International
Abstract:This study aims to experimentally investigate the influence of several key factors, including basicity, Al 2 O 3 content, TiO 2 content, SiO 2 /Al 2 O 3 ratio, and titanium reduction, on the melting properties of electric furnace slags containing titanium in the CaO–SiO 2 –MgO–Al 2 O 3 –50%TiO 2 system. The findings revealed that the melting temperature decreased with an increase in the CaO/SiO 2 ratio, Al 2 O 3 content, and SiO 2 /Al 2 O 3 ratio, while it increased with higher TiO 2 content. To achieve a low melting temperature for the slags and an appropriate phase composition for titanium extraction, it is advisable to maintain a low CaO/SiO 2 ratio within the range of 0.6–0.7, and an Al 2 O 3 content of 13% is recommended. Higher TiO 2 content is associated with elevated liquidus temperatures, while conversely, the SiO 2 /Al 2 O 3 ratio exhibits an inverse relationship. Efforts were made to limit the titanium reduction during smelting to a maximum of 0.4. Anosovite (MgTi 2 O 5 ), CaAl 2 Si 2 O 8 , Mg(Al, Ti) 2 O 4 , spinel (MgAl 2 O 4 ), augite (Ca(Mg, Fe, Al) (Al, Si) 2 O 6 ) and Ca 12 Al 14 O 33 were the primary phases in titanium slag. The calculated viscosity results align with the trends observed in the melting property results. Furthermore, the liquidus temperatures were obtained through FactSage aligns with the pattern observed in the melting temperature. These findings will serve as a valuable technical foundation to support the development of the direct reduction smelting process for the comprehensive utilization of vanadium titanomagnetite. Graphical Abstract
What problem does this paper attempt to address?