Effects of Mechanical Treatment and Pre-Deformation on Shape Recovery Stress of Ti<sub>50</sub>Ni<sub>47</sub>Fe<sub>3 </sub>shape Memory Alloy

Yu Zhang,Fu Shun Liu
DOI: https://doi.org/10.4028/www.scientific.net/msf.787.267
2014-01-01
Materials Science Forum
Abstract:Effects of mechanical treatment, pre-strain and pre-deformation temperature on shape recovery stress of Ti 50 Ni 47 Fe 3 shape memory alloys were investigated. Mechanical treatment, consisting of hot-rolling and hot-forging, improved σrmax σrmax (maximum recovery stress), dσr/dT (rate of recovery stress with temperature) and T s (the temperature at which recovery stress rises sharply). Martensitic transformation and reverse transformation temperatures also increased with increasing the hot-rolling deformation. σrmax and dσr/dT increased with increasing pre-strain at first and then decreased with further increasing of pre-strain, and the maximum values of σrmaxand dσr/dT were obtained at a pre-strain of 10%. On the other hand, σrmaxand dσr/dT decreased with increasing pre-deformation temperature. Upon a hot-rolling of 88% area reduction and pre-deformation of 10% at-150°C, the Ti 50 Ni 47 Fe 3 alloy exhibited excellent recovery stress property with the σrmax of 391MPa in combination with dσr/dT of 5.09.
What problem does this paper attempt to address?