A High Strength Near-Eutectic Al-Mg-Si Alloy Manufactured by Laser Powder Bed Fusion

Feipeng Yang,Jianying Wang,Tao Wen,Xinhai Ai,Xixi Dong,Hailin Yang,Shouxun Ji
DOI: https://doi.org/10.2139/ssrn.4250127
2022-01-01
SSRN Electronic Journal
Abstract:The traditional wrought Al-Mg-Si alloy fabricated via laser powder bed fusion (LPBF) are prone to hot cracks, unless adding special elements (Sc, Zr) or nanoparticles to alloy powder. In this work, a high strength near-eutectic Al-9.6Mg-4.9Si (Al-13.3Mg2Si) alloy with lower hot-cracking susceptibility was successfully manufactured by LPBF. The as-LPBFed near-eutectic alloy with a high relative density (~ 99.3%) was featured with fine α-Al grains and cellular eutectic Mg2Si, accompanied by a high number density dislocations, coherent GP zone and α-Al12(Fe,Mn)3Si phases. In addition to the grain refinement and dislocation strengthening, the strength enhancement (i.e. yield strength of 439 MPa, the ultimate tensile strength of 557 MPa) is mainly ascribed to the dispersion strengthening from the divorced nanosized eutectic Mg2Si. The results also demonstrate that manipulation of alloys at near eutectic composition is effective to achieve high strength Al-Mg-Si alloy processed by LPBF.
What problem does this paper attempt to address?