Formation Mechanism of Inherent Spatial Heterogeneity of Microstructure and Mechanical Properties of NiTi SMA Prepared by Laser Directed Energy Deposition

MengJie Luo,Ruidi Li,Dan Zheng,JingTao Kang,HuiTing Wu,ShengHua Deng,PengDa Niu
DOI: https://doi.org/10.1088/2631-7990/acd96f
2023-01-01
International Journal of Extreme Manufacturing
Abstract:Ni _51 Ti _49 at.% bulk was additively manufactured by laser-directed energy deposition (DED) to reveal the microstructure evolution, phase distribution, and mechanical properties. It is found that the localized remelting, reheating, and heat accumulation during DED leads to the spatial heterogeneous distribution of columnar crystal and equiaxed crystal, a gradient distribution of Ni _4 Ti _3 precipitates along the building direction, and preferential formation of Ni _4 Ti _3 precipitates in the columnar zone. The austenite transformation finish temperature ( A _f ) varies from −12.65 °C ( Z = 33 mm) to 60.35 °C ( Z = 10 mm), corresponding to tensile yield strength ( σ _0.2 ) changed from 120 ± 30 MPa to 570 ± 20 MPa, and functional properties changed from shape memory effect to superelasticity at room temperature. The sample in the Z = 20.4 mm height has the best plasticity of 9.6% and the best recoverable strain of 4.2%. This work provided insights and guidelines for the spatial characterization of DEDed NiTi.
What problem does this paper attempt to address?