Laser powder bed fusion in-situ alloying of refractory WTa alloy and its microstructure and mechanical properties

Junfeng Li,Yunxiao Wu,Lingfeng Xue,Zhengying Wei
DOI: https://doi.org/10.1016/j.addma.2023.103493
IF: 11
2023-01-01
Additive Manufacturing
Abstract:Refractory tungsten-tantalum (WTa) alloy material was prepared by laser powder bed fusion (LPBF) in-situ alloying, and the direct fabrication of WTa complex parts with good appearance and structural integrity was realized. The interior defects, phase composition, microstructure and mechanical properties of LPBF-deposited WTa alloy were investigated. The preferential combination of Ta and oxygen (O) produces an oxygen-trapping effect, which can reduce the segregation of O at the grain boundary, thereby improving the grain boundary strength and effectively suppressing the generation of intergranular cracks. The W-Ta solid solution phase was formed in LPBF-deposited WTa alloy. The solidified grains of the horizontal (XOY) and vertical (XOZ) sections are mainly striped grains with an average size of 5.18 µm and upwardly grown columnar grains with an average size of 6.43 µm, respectively. The grains of LPBF-deposited WTa alloy specimens are finer than those of LPBF-deposited W specimens. Inside the solidified grains, cellular structures with a size of around 1 µm were formed in XOY section. In the XOZ section, the transition from columnar/elongated structures at the bottom of the molten pool to fine cellular structures at the top of the molten pool was formed as a result of the varies in temperature gradients (G) and solidification rates (R). The maximum microhardness of the LPBF-deposited WTa alloy was 454.28HV0.5. The compression test showed that the ultimate compressive strength (UCS) was 1393 MPa, exhibiting a transgranular fracture mode. This study demonstrates the feasibility of in-situ fabrication of complex parts of refractory tungsten-tantalum alloy materials by LPBF.
What problem does this paper attempt to address?