Recovery of Lithium from Brine with Different Degrees of Mineralization by Resorcinol/urea–formaldehyde Foam-Supported H2TiO3

Xuezhen Wang,Xiaotong Jiang,Junmin Wu,Kaiyu Zhao,Yafei Guo,Tianlong Deng,Xiaoping Yu
DOI: https://doi.org/10.1016/j.cej.2023.142285
IF: 15.1
2023-01-01
Chemical Engineering Journal
Abstract:With the development of new energy industry, the extraction of lithium from liquid minerals has attracted extensive attention. Herein, a novel phenolic resin-supported H2TiO3 foam (RF/UF-HTO) was developed for Li+ recovery from aqueous solutions. It was found that when the thermosetting phenolic resin was modified with urea and then foamed by petroleum ether with boiling points of 60 similar to 90 degrees C under the assistance of 1.5% Tween 80 + 3% sodium dodecyl sulfate, the material presented a porous 3D network structure with a high specific surface area and porosity. The maximum adsorption capacity of the material reached 52.41 mg.g(-1). The adsorption rate was controlled by the particle diffusion, and the adsorption was proven to be an endothermic process by the microcalorimetry. The material exhibited high adsorption performance for low-concentration Li+ in geothermal water with a low degree of mineralization. The adsorption capacity reached 21.50 mg.g(-1) after only 6 h, and the attenuation of adsorption capacity was only 1.96 mg.g(-1) after 10 cycles. Because of the high Mg2+ concentration and high degree of mineralization, the adsorption capacity for Li+ in salt lake brine was low. This problem was successfully solved by regeneration with Ba(OH)(2), by which the adsorption capacity was enhanced from 0.54 to 20.72 mg.g(-1). Even for the fixed-bed adsorption, the adsorption capacity still reached 8.5 mg.g(-1). Based on these excellent properties, the material and method developed in this work can be used for Li+ recovery from brine with different degrees of mineralization and composition.
What problem does this paper attempt to address?