Insight into the Effects of Cation Disorder and Surface Chemical Residues on the Initial Coulombic Efficiency of Layered Oxide Cathode

Jin-Li Liu,Han-Feng Wu,Zhi-Bei Liu,Ying-Qiang Wu,Li Wang,Feng-Li Bei,Xiang-Ming He
DOI: https://doi.org/10.13208/j.electrochem.2219001
2022-01-01
Abstract:Lithium layered oxide LiNi0.6Co0.2Mn0.2O2(NCM622)is one of the most promising cathode materials in high-energy lithium-ion batteries for electric vehicles.However,one drawback for NCM622 is that its initial coulombic efficiency(ICE)is only about 87%,which is at least 6%lower than that of LiCoO2 or LiFePO4.In this work,we investigated the effects of surface chemical residues(e.g.,LiOH and Li2CO3)and Li/Ni cation disorder resulted during the sintering on the ICE.We found that the ICE of the as-prepared samples could be boosted from 80.80%to 86.68%as the sintering temperatures were increased from 825 to 900℃.The corresponding Li/Ni cation disorder and surface chemical residues were also reduced with the increasing sintering temperatures.Furthermore,the ICE of the sample sintered at 825℃could be enhanced by 3.57%after washing with HNO3 solution to remove the surface residues despite the Li/Ni cation disorder being increased.These results demonstrate that minimizing the amount of surface residuals and the degree of Li/Ni cation disorder through an appropriate sintering process and post-treatment technology is critical to achieve a high ICE and improve the electrochemical performances of NCM622.
What problem does this paper attempt to address?