Effect of Temperature on Coke Size and Properties of Blast Furnace

MA Shufang,YAN Liqiang,YAN Huanmin,YANG Qingbin,XUE Limin,LI Kejiang,ZHANG Jianliang,WU Shengli
DOI: https://doi.org/10.19864/j.cnki.jxye.2022.06.001
2022-01-01
Abstract:At present, the iron-making industry has increasingly higher requirements for the quality of coke. It is very important to clarify the deterioration mechanism of the coke in the blast furnace and to reasonably control the quality of the coke to ensure the stability of the blast furnace. High temperature is the first physical environment that coke faces after entering the blast furnace, which has an obvious influence on the structure and properties of coke. In this paper, the influence of temperature on coke lumpiness and properties was studied through the macroscopic analysis of indicators such as coke weight loss rate, and observation of the microstructure of coke cracks and pores by industrial computed tomography(CT). The results show that no obvious change in the inner structure of the coke is detected at 1 100 ℃. With the temperature rising to 1 300 ℃, the internal crack length of coke increases slightly. When the annealing temperature is 1 500 ℃, the coke crack is further extended, the pore size increases, and some micro-pores are connected to form microcracks. Regarding the further reaction mechanism of coke with gas and liquid phases in the blast furnace under high temperature conditions, more in-depth experimental and theoretical studies are needed.
What problem does this paper attempt to address?