Quantitative Evaluation Process Practice of Residual Oxygen in Tundish

Zhang Hejun,Meng Qingyong,Shan Qinglin,Pan Hongwei,Tang Guangpeng,Lu Boxun,Zhang Shijun,Wen Juwen,Lei Ming
DOI: https://doi.org/10.3969/j.issn.1009-7864.2022.05.008
2022-01-01
Abstract:During continuous casting, the residual oxygen in tundish may cause the secondary oxidation of molten steel, restrict the purity improvement of molten steel.By means of improved residual oxygen measuring device to determine the residual oxygen content in the 70 t tundish of Tangsteel New District, quantitative analysis is carried out on the effects of the tundish cover sealing state, the fan on and off condition, argon blowing flow rate through tundish cover on residual oxygen content.Under the sealing condition of the tundish cover opening, the residual oxygen content in tundish can be stablely controlled below 0.5% by taking measures of switching off the fan on the platform and increasing the argon flow rate to 5 000 L/min.After adding argon blowing branch piping at the long nozzle of tundish cover, the residual oxygen content in tundish can be further reduced below 0.008%,which shall provide better shrouded pouring condition during casting.
What problem does this paper attempt to address?