Abstract:Spiral fibers were considered to be an ideal toughening phase of ultra-high torsional release effect. In this work, ZrB2 (Z)-20 vol% SiC (S) spiral fiber (ZS(sf)) with controllable structure was prepared by a combination approach of liquid rope effect and non-solvent-induced phase separation. Dominantly depended on the kinematic viscosity (.), dropping height (H), and flow rate (Q), the geometric parameters of ZSsf involving filament diameter (d) and coil diameter (D) were followed the relationship of d approximate to 0.516x10(-3)Q(1/2)H(-1/4) and D approximate to 0.25x10(-3)(Q/H)(1/3), respectively, within the optimized. of 10-15 Pa center dot s. Three different microstructures of ZS(sf) were achieved by adjusting the polymer/solvent/ non- solvent system assisted with phase diagram calculation, including dense, hollow, and hierarchical pore structures. The ZrB2-SiC with 1 wt% ZS(sf) composites prepared by hot isostatic pressing (HIP) exhibited a similar to 30% increase in fracture toughness (K-IC, 4.41 MPa center dot m(1/2)) compared with the ZrB2-SiC composite, where the microscopic fracture toughness of the ZS(sf) was similar to 80% higher than that of the matrix. The fibers with a similar to 10 nm in-situ-synthesized graphite phase amongst grain boundaries of ZrB2 and SiC changed the fracture mode, and promoted the crack deflection and pull-out adjacent the interface of matrix and the fiber.
What problem does this paper attempt to address?