Hot tensile deformation behaviour and microstructure evolution of Al3La phase reinforced Mg-5Li-3Al-2Zn alloy formed in-situ by La2O3 particle

Xiaoqiang Li,Qichi Le,Chenglu Hu,Tong Wang,Wenxin Hu,Lei Bao,Ping Wang,Dandan Li,Xiong Zhou
DOI: https://doi.org/10.1016/j.matchar.2022.111772
IF: 4.537
2022-01-01
Materials Characterization
Abstract:In this study, LAZ532 alloy reinforced with Al3La phase in-situ precipitated by adding La2O3 particle was fabricated by melting casting. The hot tensile deformation behaviour of the composite was investigated at deformation temperatures of 423 K ~ 573 K and strain rates of 8.3 × 10−5 s−1–1.7 × 10−3 s−1. The results indicated that the peak stress and elongation at fracture of the composite gradually decreased and increased respectively, with the deformation temperature increased or the strain rate decreased. In particular, the composite exhibited outstanding quasi-superplasticity with elongation to fracture up to 213% at 573 K and 8.3 × 10−5 s−1. Based on the results of theoretical calculation, the activation energy Q of the composite was 97.8 kJ/mol. In addition, by the observation and analysis of microstructure at different strains, the strain induced the precipitation of pearlite-like Al3La phase in the grains during hot tensile deformation. The deformation behaviour of the composite was a synergetic deformation mechanism dominated by GBS, supplemented by DDRX and intragranular slip, and the intragranular slip was dominated by prismatic and pyramidal I <c+a> slips.
What problem does this paper attempt to address?