Surface Morphology of La<Subscript>1.85</Subscript>Sr<Subscript>0.15</Subscript>CuO<Subscript>4</Subscript>/LaSrGaO<Subscript>4</Subscript>(100) Films Deposited by laser Ablation at Different Oxygen Pressures

C. Buzea,H. B. Wang,S. J. Kim,T. Tachiki,Y. Uematsu,K. Nakajima,T. Yamashita
DOI: https://doi.org/10.1007/978-4-431-66877-0_288
2000-01-01
Abstract:The film surface morphology of LSCO films deposited by laser ablation gives information related to the velocity of the ablated species during deposition. We noticed a change in the shape of the grains as follows: at 396 mTorr oxygen pressure, the grains embody a tubular-ellipsoid form; at 230 mTorr the shape changes into a parallelepiped-type with flattened edges, one side flatter than the other; for 176 mTorr the shape becomes a “corn grain” type. These results suggest the speed of the ablated clusters is higher for low oxygen pressures, as demonstrated by the aerodynamic form of the grains.
What problem does this paper attempt to address?