Sinter-joining of W-10Ti Powder to W-10Ti Waste Target by Spark Plasma Sintering

Lei Huang,Yafei Pan,Jiuxing Zhang,Wenfei Xu,Yong Du,Yuhui Zhang,Shuyan Zhang
DOI: https://doi.org/10.1016/j.mtcomm.2021.102372
IF: 3.8
2021-01-01
Materials Today Communications
Abstract:Spark plasma sintering (SPS) technology has been applied to the sinter-joining of W-10Ti powders and W-10Ti waste targets. The effects of joining temperature (1200-1600 degrees C) and time (5-20 min) on the microstructure evolution and mechanical properties were studied systematically. The microstructural observation results indicated that the joining temperature and time had a significant effect on the number of beta Ti(W) phase and grain size. There was little difference in the distribution of relative density and hardness between the powder-sintered body and waste target. The bending strength of the original waste target and regenerated target (1500 degrees C/5 min) was 660.32 +/- 18.94 MPa and 455.30 +/- 15.12 MPa, indicating that the powder-sintered body and the waste target achieved a good joining when the temperature was 1500 degrees C and the time was 5 min. A regenerated W-10Ti target with reliable interface joining, high density, less beta Ti(W) phase and small grain size was obtained at the joining temperature of 1500 degrees C and the dwelling time of 5 min. EBSD results at 1500 degrees C/5 min suggested that the grain boundary diffusion induced the formation of wedge-shaped triple junctions and that a reconstruction behavior occurred at the interface. A schematic diagram was established to characterize the mechanism of the interface formation and evolution. The series of sinter-joining processes assisted by SPS technology are considered to involve pressure welding, micro-arc welding, resistance welding and diffusion welding, which can provide experimental reference and theoretical guidance for repairing the W-10Ti waste target with SPS technology.
What problem does this paper attempt to address?