Abstract:In order to solve corrosion problem of heat exchanger metal materials in waste heat utiliza-tion of low-temperature flue gas of steel furnaces, low-temperature corrosion resistance properties of five metal materials were studied using self-design test rig, the wall thickness testing, thickness and element of corrosion layer was detected by SEM and EDS, and the corrosion mechanism of metal mate-rials was analyzed in detail.The results show that in the flue gas of rolling steel heating furnace, 20g steel and ND steel has serious corrosion, and corrosion resistance properties of ND steel is higher than20g.Corrosion of three kinds of stainless steel has little difference and they haven't evident corro-sion.From the microscopic results, the corrosion resistance of stainless steel in order is 316L>316>304, and the corrosion rate is 35-190μm/a, and the main reason that causes corrosion of these mate-rials is acid dew corrosion.
What problem does this paper attempt to address?