Thermodynamic analysis on iron-making process of zinc leaching residue by carbon reduction

LIU Yang,TAN Jun,LIU Chang-qing,YIN Zhou-lan,CHEN Qi-yuan,ZHANG Ping-min,LIAO Zhou
DOI: https://doi.org/10.19476/j.ysxb.1004.0609.2015.07.030
2015-01-01
The Chinese Journal of Nonferrous Metals
Abstract:Iron-making of zinc leaching residue was obtained by carbon reduction in bath smelting, and the thermodynamic process was analyzed. The results show that Fe2O3is the pyrolysis product of ZnFe2O4 and KFe3(SO4)2(OH)6. ZnFe2O4 can not decompose in the temperature range of 300?1800 K, but KFe3(SO4)2(OH)6 decomposes at 652.25K. HigherpCO/pCO2and lower temperature that should be higher than the slag melting temperature, are favor able to the reduction of Fe2O3. The metal sulfates of K2SO4and CaSO4 are decomposing products of sulfur-contained phases at low temperature, and the favorable desulfurization conditions of K2SO4and CaSO4 are high temperature, low sulfur-partial pressure and low oxygen-partial pressure that must be higher than the limit of sulfates converting into sulfides. The desulfurization of CaSO4 is easier than that of K2SO4. CaO in zinc leaching residue reduces the initial reaction temperature of Zn2SiO4reduction, improves slag basicity and activity of CaO in slag and decreases the sulfur distribution ratio between liquid iron and molten slag.
What problem does this paper attempt to address?