Calculation of Stress Intensity Factor in Typical Fatigue Assessment for Container Ships

Fan LIU,Xiaoping HUANG
DOI: https://doi.org/10.3969/j.issn.1000-4882.2015.01.004
2015-01-01
Abstract:In the fatigue crack growth theory based fatigue assessment method, fatigue hot spots need to be identified and stress intensity factor of crack should be determined accurately. In this paper, fatigue assessment nodes defined in CCS Standard are divided into four categories: weld toe of butt-joints and T-joints, bottom plate of bracket toe, bracket plate of bracket toe, and intersection point of three perpendicular components. The SIFs of surface cracks at the first three categories are analyzed with 3D FEA and compared with the results of SIF magnification factors calculated with equations recommended in BS7910.The results show that the SIF magnification factors of surface crack at first category is close to that of BS7910, while the results of second and third categories are quite different from BS7910. Correction formulas are proposed respectively for second and third categories, and the results show well agreement with that from FEA.
What problem does this paper attempt to address?