AN EXPERIMENTAL STUDY ON FRACTAL PORE SIZE DISTRIBUTION AND HYDRO-MECHANICAL PROPERTIES OF GRANITES AFTER HIGH TEMPERATURE TREATMENT

Richeng Liu,Hongwen Jing,Xiaozhao Li,Qian Yin,Zengguang Xu,Ming He
DOI: https://doi.org/10.1142/s0218348x21500833
2020-01-01
Fractals
Abstract:This study experimentally estimated the fractal pore size distribution of granites, which is then linked to the hydro-mechanical properties of rocks treated by temperatures that range from 25[Formula: see text]C to 900[Formula: see text]C. The mercury intrusion experiment was carried out to characterize the pore size distributions and the MTS815.02 triaxial testing system was used to investigate hydro-mechanical properties of rocks. Finally, the micro-CT scanning system and scanning electron microscope system were employed to exhibit the evolutions of microstructures of cracks that were then linked to the macroscopic hydro-mechanical properties. The results show that the pore size distribution of granites follows the fractal scaling law and the fractal dimension ranges from 2.45 to 2.94. The fractal dimension decreases significantly when the temperature increases from 25[Formula: see text]C to 100[Formula: see text]C and then holds a constant with continuously increasing the temperature to 400[Formula: see text]C. The fractal dimension slightly increases as the temperature increases from 400[Formula: see text]C to 500[Formula: see text]C and decreases following a linear relationship until the temperature of 900[Formula: see text]C. The porosity obtained by the mercury intrusion experiment shows an exponential relationship with the fractal dimension. Both the axial stain and peak total stain, as well as the initial permeability and the permeability at the peak axial stress, have quadratic functions with the fractal dimension. The mean aperture of fractures increases from 56.75[Formula: see text][Formula: see text]m to 76.10[Formula: see text][Formula: see text]m with increasing the temperature from 100[Formula: see text]C to 900[Formula: see text]C through micro-CT scanning. The scanning electron microscope test clearly shows that the fractures are generated when the temperature exceeds 300[Formula: see text]C, which agrees well with the micro-CT scanning results. With increasing the temperature from 400[Formula: see text]C to 900[Formula: see text]C, both the number and aperture of fractures increase, which well interprets that both the strain and permeability increase as indicated by the triaxial stress-flow tests.
What problem does this paper attempt to address?