Low-Cost Preparation of YSZ-SiC High-Temperature Composite from Zircon and Y2O3 by Carbothermal Reduction

Xu Youguo,Yin Li,Guan Ming,Chen Haibo,Fang Minghao,Liu Yangai,Huang Zhaohui
2013-01-01
Rare Metal Materials and Engineering
Abstract:YSZ-SiC composite powders were synthesized by carbothermal reduction of zircon with 8 mol% Y2O3. The YSZ-SiC composite matrix was prepared by pressless sintering using the YSZ-SiC composite powders in air and Ar separately. The effect of heating temperature and 8 mol% Y2O3 on the phase compositions and microstructure of products by carbothermal reduction of zircon was investigated. The influence of sintering atmosphere on the bulk density and flexural strength of the composite matrix was discussed. The results show that the optimum temperature for synthesizing YSZ-SiC composite powders by carbothermal reduction of zircon with 8 mol% Y2O3 is 1550 degrees C and the main phases in the products are c-ZrO2 and beta-SiC. The bulk density and flexural strength of the samples sintered in air are 3.58 g/cm(3) and 91.9 MPa respectively, while they are 3.07 g/cm(3) and 58.9 MPa respectively when sintered in Ar. The phases of the samples sinterd in air are zircon and c-ZrO2, while they are c-ZrO2 and beta-SiC in Ar.
What problem does this paper attempt to address?