Preparation and Properties for (SiC)Cf/Si3 N4 Composite

Weiling XIAO,Peng XIAO,Wei ZHOU,Heng LUO,Yang LI
DOI: https://doi.org/10.3969/j.issn.1007-2330.2015.03.008
2015-01-01
Abstract:SiC coating modified C f by CVD, then fabricated (SiC)C f / Si3N4 composite by gelcasting. The effect of (SiC)C f content toward the mechanical and absorbing properties of the composite were investigated. The flexure strength of (SiC)C f / Si3N4 composites reduced 112 MPa compare with Si3N4 ceramic and the fracture toughness increase 11. 5 MPa·m / 2 when the (SiC)C f content is 10wt% , meanwhile both the real (ε') and imaginary (ε′′) permittivity of (SiC)C f / Si3N4 composite ceramics reached maximum, the dielectric constant ε' is about 15 to 18 and ε′′ is about 6 to 8; the reflectivity of the composites moved to a lower frequency with the (SiC)C f content and thickness increased.
What problem does this paper attempt to address?