Purification Technique of Regenerated Magnesium Alloy Melt

ZHANG Jun,HE Liang-ju,LI Pei-jie
DOI: https://doi.org/10.3321/j.issn:1001-4977.2005.07.007
2005-01-01
Abstract:The relationship between time and content and size of inclusions in regenerated magnesium alloy melt is researched. The rules of content changes of main alloy components and impurity elements are studied. The relationship between deposition distance and time is simulated by Stokes equation. The influence factors of deposition velocity of inclusion are analyzed. The results show that the inclusion content could be reduced less than 0.5% and inclusion size could be reduced less than 0.3mm if the melt is stewed for 5 to 10 minutes after fusion completely. The refining effect of 234 flux is better than RJ-1 flux. The inclusion content could be reduced less than 0.02% if the melt is stewed for 8 minutes after refined by 234 flux and inclusion size could be reduced less than 10μm. The deposition velocity of inclusion is directly proportional to its square diameter and density, and inversely proportional to melt viscosity coefficient and the ratio of melt density and inclusion density.
What problem does this paper attempt to address?