Joints of Continuous Carbon Fiber Reinforced Lithium Aluminosilicate Glass Ceramics Matrix Composites to Ti60 Alloy Brazed Using Ti-Zr-Ni-Cu Active Alloy

Shengpeng Hu,Dongdong Feng,Long Xia,Ke Wang,Renwei Liu,Zhentao Xia,Hongwei Niu,Xiaoguo Song
DOI: https://doi.org/10.1016/j.cja.2018.07.006
IF: 5.7
2018-01-01
Chinese Journal of Aeronautics
Abstract:Continuous carbon fiber reinforced lithium aluminosilicate glass ceramics matrix composites (C-f/LAS composites) are joined to Ti60 alloy vacuum brazed using Ti-Zr-Ni-Cu brazing alloy. The effects of the brazing temperature on the interfacial microstructure and mechanical properties of brazed joints are investigated in details. The interfacial microstructure varies apparently with an increase of the brazing temperature. The thicknesses of the banded Ti solid solution (Ti(s, s)) and the reactive layer between C-f/LAS composites and the interlayer grow gradually. The mechanical properties of brazed joints increase firstly and then decrease with an increasing temperature. In addition, a joint that is brazed at 980 degrees C for 10 min shows the highest shear strength of similar to 38.13 MPa. At the same time, the fracture paths of brazed joints also change as the temperature increases. When the brazing temperature is 950 degrees C, the fracture position is in the TiC + ZrC + Ti2O + ZrSi2 + Ti5Si3 layer on the composite side. When the brazing temperature is 980 degrees C, the fracture position is on the side of the braze seam (Ti, Zr)(2)(Ni, Cu), Ti2O + ZrSi2 + Ti5Si3 layer, and carbon fiber in the composite material. When the brazing temperature is 990 degrees C, the fracture position is in the Ti2O + ZrSi2 + Ti5Si3 layer on the composite side and the carbon fiber in the composite material. (C) 2018 Chinese Society of Aeronautics and Astronautics. Production and hosting by Elsevier Ltd.
What problem does this paper attempt to address?