Microstructure and mechanical properties of C/C composite joint brazed with Ni-based filler

He-li PENG,Yong-xin ZHANG,Xu CHEN,Hong-qiang ZHANG,Jun-liang XUE,Wei GUO
DOI: https://doi.org/10.1016/s1003-6326(22)65843-6
IF: 3.752
2022-03-01
Transactions of Nonferrous Metals Society of China
Abstract:The novel Ni-based brazing filler was used to join C/C composites. When brazing temperature increased from 1080 to 1100 °C, the wetting angle decreased from 23° to 14°, and the brazing filler had good wettability on the surface of C/C composites. The brazing seam of the brazed joint consisted of Ni(s,s) and Cr3C2 phases. As brazing temperature increased, lots of Cr3C2 phases were generated at the bonding interface, and the thick reaction layer was formed. When brazing temperature was 1120 °C, the shear strength of C/C joint reached the maximum value of 31.5 MPa. The fracture path extended in the C/C matrix close to the bonding interface.