Effect of annealing temperature on coercivity of Nd-Fe-B magnets with TbFeAl doping by process of hot-pressing

Ze-Teng Shu,Bo Zheng,Guang-Fei Ding,Shi-Cong Liao,Jing-Hui Di,Shuai Guo,Ren-Jie Chen,A-Ru Yan,Lei Shi
DOI: https://doi.org/10.1088/1674-1056/ab7b57
2020-01-01
Abstract:The Nd-Fe-B magnets are pre-sintered and then processed with hot-pressing, and the resulting magnets are called the hot-pressed pretreated (HPP) magnets. The coercivity of the HPP magnets increases as the annealed temperature increases. When the annealing temperature is 900 degrees C, the coercivity of the magnet is only 17.6 kOe (1 Oe = 79.5775 A.m(-1)), but when the annealing temperature rises up to 1060 degrees C, the coercivity of the magnet reaches 23.53 kOe, which is remarkably increased by 33.7%. The microstructure analysis indicates that the grain surface of the HPP magnet becomes smoother as the annealed temperature increases. The microstructure factor alpha is changed according to the intrinsic coercivity model formula. The alpha of the magnet at 900 degrees C is only 0.578, but it is 0.825 at 1060 degrees C. Microstructural optimization is due mainly to the increase of coercivity of the HPP magnet.
What problem does this paper attempt to address?