Growth and Piezoelectric Properties of Large Size Ca3Ta(Ga0.5Al0.5)3Si2O14 Crystals with Langasite Structure

Kainan Xiong,Sheng Wang,Xiaoniu Tu,Yanqing Zheng,Tomoaki Karaki,Erwei Shi
DOI: https://doi.org/10.1016/j.jcrysgro.2020.125525
IF: 1.8
2020-01-01
Journal of Crystal Growth
Abstract:4 in. Ca3Ta(Ga0.5Al0.5)3Si2O14 (CTGAS) in which 50% of Ga replaced by Al in Ca3TaGa3Si2O14 (CTGS) crystal has been successfully grown by Czochralski technique. The full width at half-maximum (FWHM) of the rocking curves of five regions of CTGAS are found to be from 17.6″ to 18.2″. All the effective segregation coefficients Keff of chemical compositions are very close to 1. At room temperature, the piezoelectric coefficients d11 and d14 of CTGAS are found to be 3.96 pC/N and −2.21 pC/N, and the electromechanical coupling coefficients k12 and k26 are determined as 9.3% and 29.9%, respectively. In the range from 500 °C to 800 °C, the X-cut of as-grown crystal possesses high electric resistivity. And the transmittances of CTGAS crystal are over 80% from 700 nm to 2700 nm.
What problem does this paper attempt to address?