High-Softening-Point Pitches Prepared By The Br-2 Modification Of Low-Temperature Coal Tar Pitch And Their Mesophase Transformation Behavior

Yang Hai-Xiao,Han He-Xiang,Wang Ji-Tong,Qiao Wen-Ming,Ling Li-Cheng
DOI: https://doi.org/10.1016/j.carbon.2019.04.099
IF: 10.9
2019-01-01
Carbon
Abstract:High-softening-point pitches were prepared from refined low-temperature coal tar pitch (R-CTP) by thermal bromination, followed by dehydrobromination/polymerization. R-CTP was first brominated in the presence of 5-20 wt.% bromine, and then heat-treated at 250-350 degrees C for dehydrobromination/polymerization. The structures of the dehydrobrominated pitches were characterized by 1H NMR, LDI-TOF/MS and FT-IR. The introduction of bromine significantly facilitated polycondensation of the component molecules and Br-2 modification apparently increased the softening point, coking values and molecular weight of the obtained pitches compared with that formed by direct thermal condensation. The dehydrobrominated pitches showed relatively low melt viscosities and shearing-thinning rheological behavior with obvious plateau regions. An optimized dehydrobrominated pitch produced from R-CTP modified with 15 wt.% bromine (BRC-15% ) by heat-treatment at 350 degrees C for 6 h had a softening point of 232 degrees C and a carbon yield of 55. 2 wt.% . Polarized optical microscopy showed that the semicoke produced by the carbonization of BRC-15 % at 410 degrees C appeared to be the most anisotropic with a large domain texture, and XRD patterns indicated that this sample also had the largest crystallite size ( L-c = 117 angstrom) of all samples examined.
What problem does this paper attempt to address?