Microstructure and Mechanical Properties at Elevated Temperature of Laser-Welded Ti–22Al–25Nb Alloy Sheets

Beibei Kong,Dongjun Wang,Faye Zang,Kehuan Wang,Gang Liu
DOI: https://doi.org/10.1016/j.intermet.2019.106516
2019-01-01
Abstract:The tensile tests of laser-welded Ti-22Al-25Nb alloy with a transverse joint are carried out in temperatures ranging from 850 degrees C to 930 degrees C. The result showed that 875 degrees C was a critical temperature. The critical temperature could determine the fracture mode of welded samples due to the microstructural differences between the fusion zone and base metal. Fracture occurred in the welded joint when deformation temperature was less than 875 degrees C, while it occurred in base metal in temperature range 880-930 degrees C. Besides, volume fraction of spherical and strip like alpha(2)/O grains in the fusion zone decreased with increasing temperature, and long axes of the strip-like grains showed a certain angle with respect to beta/B2-phase grain boundaries. These strip-like grains impeded crack nucleation and propagation to some extent.
What problem does this paper attempt to address?