Mg(Ti0.95Sn0.05)O3–(Ca0.8Sr0.2)TiO3 Ceramics: Phase, Microstructure, and Microwave Dielectric Properties

Javed Iqbal,Hanxing Liu,Hua Hao,Atta Ullah,Minghe Cao,Zhonghua Yao,Abdul Manan
DOI: https://doi.org/10.1016/j.jallcom.2018.01.297
IF: 6.2
2018-01-01
Journal of Alloys and Compounds
Abstract:The phase, microstructure, and microwave dielectric properties of (1 - x)Mg(Ti0.95Sn0.05)O-3-x(Ca0.8Sr0.2)TiO3 (0.01 <= x <= 0.07) ceramics were investigated. (Ca0.8Sr0.2)TiO3 was used as a tau(f) compensator and was added to Mg(Ti0.95Sn0.05)O-3 to obtain a temperature-stable material. The powder X-ray diffraction patterns suggest the presence of Mg(Ti0.95Sn0.05)O-3 as the main crystalline phase and Ca0.8Sr0.2TiO3 and MgTi2O5 as the minor phases. With increasing (Ca0.8Sr0.2)TiO3 content, the dielectric constant epsilon(r) and the temperature coefficient of the resonant frequency tf of the ceramics increases, whereas the unloaded quality factor Q(u)f(o) decreases. For 0.95[Mg(Ti0.95Sn0.05)O-3]-0.05(Ca0.8Sr0.2)TiO3 ceramics sintered at 1375 degrees C, the dielectric constant epsilon(r) (21.1), the quality factor Q(u)f(o) (117,000) at 9 GHz, and the temperature coefficient of the resonant frequency tau(f) (-1.79 ppm/degrees C) were obtained. (C) 2018 Elsevier B.V. All rights reserved.
What problem does this paper attempt to address?