Microwave Dielectric Properties of (1-x)(Ca0.61Nd0.26)TiO3–x(Li0.5Sm0.5)TiO3

wei wang,zi long tang,zhong tai zhang
2007-01-01
Key Engineering Materials
Abstract:(1-x)(Ca0.61Nd0.26)TiO3-x(Li0.5Sm0.5)TiO3 (0.2 <= x <= 0.7) ceramics were prepared by solid-state reaction rnethod and the microwave dielectric properties of the resultant materials at different (Li0.5Sm0.5)TiO3 contents were investigated. A single phase of perovskite in all samples was confirmed by XRD patterns. With increasing (Li0.5Sm0.5)TiO3 content, Q x f value and dielectric constant (epsilon(r)) decrease slightly and the temperature coefficients of the resonant frequency (tau(f)) of the specimens decreases noticeably. The optimum parameters, i.e., epsilon(r) = 109, Q x f = 5259 GHz and tau(f) = similar to 0 ppm/degrees C, for the composition of 0.4(Ca(0.61)Ndo(0.26))TiO3-0.6(Li0.5Sm0.5)TiO3 was obtained when keep the calcination temperature at 1250 degrees C for 3 h.
What problem does this paper attempt to address?