The study on surface modification process of nanometer CeO2

Zhen HU,Li-qun XIE,Chang-nan YANG,Yan ZHAO,Yan-ping LI
DOI: https://doi.org/10.3969/j.issn.1008-0511.2007.03.006
2007-01-01
Abstract:The sodium laurate was used to modificate the nanometer CeO2 which was prepared in this work.At first all the effect factors were investigated respectively and each optimum range of factors was obtained.Because of cross action between the four factors,the orthogonal tests were done in order to obtain the optimum condition of modification.The modifier concentration was 2.1 g/L,the modification temperature was 45 ℃,the modification pH was 6 and modification time was 18 min.The lipophilicity of the nanometer CeO2 which was modified under optimum condition was 0.48.The powders were well dispersed in alcohol.