Enhanced Micro-Hardness and Wear Resistance of Al-15Si/TiC Fabricated by Selective Laser Melting

Yan Zhou,Longchen Duan,Shifeng Wen,Qingsong Wei,Yusheng Shi
DOI: https://doi.org/10.1016/j.coco.2018.06.009
IF: 8
2018-01-01
Composites Communications
Abstract:High relative density (> 98%) Al-15Si alloy samples were fabricated by selective laser melting (SLM) with laser re-melting process. The micro-hardness and wear resistance of Al-15Si alloy samples were investigated in this study. The addition of 5 wt% TiC improved the micro-hardness of SLM-produced Al-15Si alloy, which had a remarkable micro-hardness of 172.8 Hv. After the heat treatment (annealing or quenching), the hardness of all tested samples decreased significantly, while the Al-15Si/TiC composites with the laser re-melting kept the higher hardness values (145 Hv). This sample presented the lower coefficient of friction (0.42) and wear rate (2.75 x 10(5) mm(3) N-1 m(-1)) than other conditions. Based on the results, the addition of 5 wt% TiC with laser remelting in SLM process, together with annealing treatment afterwards, was a feasible approach to obtain a high micro-hardness and good wear resistance of Al-15Si alloys.
What problem does this paper attempt to address?