Core Loss Analysis of Finemet Type Nanocrystalline Alloy Ribbon with Different Thickness

Zhun Li,Kefu Yao,Deren Li,Xiaojun Ni,Zhichao Lu
DOI: https://doi.org/10.1016/j.pnsc.2017.09.002
IF: 4.269
2017-01-01
Progress in Natural Science Materials International
Abstract:Nanocrystalline soft magnetic materials are widely used in power electronic applications due to their high permeability, magnetization and low core loss. In this paper, Fe73.5Cu1Nb3Si15.5B7 (at%) nanocrystalline alloy ribbons, with ultra-thin thickness of 14µm, and also 18 and 22µm, were prepared by a planar flow casting method with a single roller device. Soft magnetic properties of these ribbons were analyzed after nanocrystallization annealing. The experiments were conducted on toroidal samples using IWATSU B-H Analyzer over a frequency range of 10–100kHz, at induction amplitudes of 100–500mT, at room temperature. It was found that the excess eddy current loss Pex was the dominant factor in the overall core loss above 10kHz. The toroidal samples made of the 14µm thickness ribbon exhibit very low total core loss of 48W/kg at a frequency of 100kHz and magnetic flux density of 300 mT. The ratio of the Pex was up to 89% at 100kHz. The ribbon with lower thickness exhibits lower Pex and therefore lower total core loss. The domain structure evidences were found. It indicates that the ribbons with small thickness are preferable for application in high frequency condition.
What problem does this paper attempt to address?