Preparation of Coating Material of Welding Electrode from Marine Placer Via Carbothermic Reduction

Tu Hu,Xuefeng Liao,Jie Li,Jinhui Peng,Libo Zhang,Li Yang,Zhaogang Li
DOI: https://doi.org/10.2355/isijinternational.isijint-2016-663
2017-01-01
ISIJ International
Abstract:The preparation of coating material of welding electrode from marine placer via carbothermic reduction was systematically investigated. Four stages were observed in the carbothermic reduction of marine placer-coal mixture. The release of the volatiles in coal occurred at the first stage (<= 600 degrees C), and the solid solid reduction and gas-solid reduction occurred at the second (600-960 degrees C) and third stages (960-1 350 degrees C), respectively. The reduction rate of iron oxide at the third stage was higher than that at the second stage because of the high carbon gasification rate. A slowdown in the total mass loss at approximately 1 350 degrees C occurred at the fourth stage. X-ray diffraction patterns show that the reduction process of the marine placer exceeded 1 100 degrees C and can be written as: FeTiO3 -> FeTi2O5 -> Fe+FTiO2. The quality index of the reduced ilmenite was evaluated in terms of the TiO2 and Feo content. The TiO2 content gradually increased as the reduction temperature increased from 1 000 degrees C to 1 300 degrees C, and the reduction time exerted lesser influence than temperature. The FeO content initially decreased rapidly and then exhibited a downward trend that became slower after 120 min with increasing reduction time. The TiO2 index could be achieved easily because of the high TiO2 content of the raw material. The FeO content could reach 8.45% after reduction at 1 300 degrees C for 180 min, which exceeded the technical requirement of 9%.
What problem does this paper attempt to address?