Effects of the Be 22 W Phase Formation on Hydrogen Retention and Blistering in Mixed Be/W Systems

Jin-Li Cao,Bing-Ling He,Wei Xiao,Li-Gen Wang
DOI: https://doi.org/10.1088/1674-1056/26/7/076801
2017-01-01
Abstract:We have performed first-principles density functional theory calculations to investigate the retention and migration of hydrogen in Be22W, a stable low-W intermetallic compound. The solution energy of interstitial H in Be22W is found to be 0.49 eV lower, while the diffusion barrier, on the other hand, is higher by 0.13 eV compared to those in pure hcp-Be. The higher solubility and lower diffusivity for H atoms make Be22W a potential beneficial secondary phase in hcp-Be to impede the accumulation of H atoms, and hence better resist H blistering. We also find that in Be22W, the attraction between an interstitial H and a beryllium vacancy ranges from 0.34 eV to 1.08 eV, which indicates a weaker trapping for hydrogen than in pure Be. Our calculated results suggest that small size Be22W particles in hcp-Be might serve as the hydrogen trapping centers, hinder hydrogen bubble growth, and improve the resistance to irradiation void swelling, just as dispersed oxide particles in steel do.
What problem does this paper attempt to address?