Effects of heat treatment on microstructure evolution and mechanical properties of Mg-6Zn-1.4Y-0.6Zr alloy

Jing Wang,Xiao-gang Fang,Shu-sen Wu,Shu-lin Lü
DOI: https://doi.org/10.1007/s41230-017-6075-5
2017-01-01
China Foundry
Abstract:To investigate the effects of solution temperature and the decomposition of I-phase on the microstructure, phase composition and mechanical properties of as-cast Mg-6Zn-1.4Y-0.6Zr alloy, solution treatment at 440 ºC, 460 ºC and 480 ºC and further aging treatment were conducted on the alloy. The results indicate that the net-like intermetallic compounds (mainly I-phase) dissolve into the α-Mg matrix gradually with the increase of solution temperature from 440 ºC to 480 ºC. Besides, the I-phase decomposes completely at 480 ºC, with the formation of fine W-phase (thermal stable phase) and Mg 7 Zn 3 phase. In addition, a great number of fine and dispersive Mg-Zn binary phases precipitate in the α-Mg matrix during the aging treatment. Due to the increase of solute atoms and the precipitation of strengthening phases, such as W-phase and Mg-Zn phases, the optimal strength is obtained after solution treatment at 460 ºC for 8 h and aged at 200 ºC for 16 h. The yield strength (YS), ultimate tensile strength (UTS) and elongation are 208 MPa, 257 MPa and 3.8%, respectively. Compared with the as-cast alloy, the increments of YS and UTS are 117% and 58%, respectively, while the decrement of elongation is 46%.
What problem does this paper attempt to address?