Abstract:A new type of thermally sensitive fibers with an antimony selenide (Sb2Se3) core and phosphate glass cladding is demonstrated. The fibers were fabricated by a molten core method and maintained overall diameters ranging from 250 to 800 mu m and core diameters of 35-200 mu m. A 2.8 cm long Sb2Se3 core fiber, electrically contacted to external circuitry through fiber end facets, exhibited a four orders of magnitude change in conductivity after the whole fiber was heated from 25 to 195 degrees C. In addition, the fiber exhibited enhanced photoconductivity under illumination. These results indicate that Sb2Se3 core multimaterial fibers have promising applications in temperature sensing, optical switches and photodetectors. (C) 2016 Elsevier B.V. All rights reserved.