Unusual effects of vacuum annealing on large-area Ag3PO4 microcrystalline film photoanode boosting cocatalyst- and scavenger-free water splitting
Qi Cao,Jun Yu,Yue Cao,Jean-Jacques Delaunay,Renchao Che
DOI: https://doi.org/10.1016/j.jmat.2021.04.003
IF: 8.589
2021-09-01
Journal of Materiomics
Abstract:Large-area Ag<sub>3</sub>PO<sub>4</sub> film photoanodes are obtained and annealed in vacuum for OER.400 ºC is the critical temperature for .|Recovery|–|Recrystallization| process during annealing.400 ºC-annealed photoanode shows much improved crystal quality and light absorbance.400 ºC-annealed photoanode shows 88% increase in current density than non-annealed one.Drastically improved stability of the 400 ºC-annealed photoanode is also demonstrated.Ag<sub>3</sub>PO<sub>4</sub> as a novel photoanode material, despite its arguably highest photoactivity, suffers for its poor light absorption and stability for photoelectrochemical (PEC) water oxidation. In this work, 4.5×4.5 cm<sup>2</sup> Ag<sub>3</sub>PO<sub>4</sub> microcrystalline films are grown <em>via</em> a room-temperature solution process, and vacuum annealing is proposed to solve the stability and light absorption issues. It is found that the major process below 400 ºC of vacuum annealing is the |Recovery| process for Ag<sub>3</sub>PO<sub>4</sub> microcrystals, when lattice defects and Ag<sup>0</sup> surface species get reduced. Next, |Recrystallization| stage occurs at >400 ºC. The recovery of native defects of silver vacancies, with both density functional theory calculation and experimental results, could simultaneously improve the light absorption and catalytic activity of Ag<sub>3</sub>PO<sub>4</sub>. The 400 ºC-annealed Ag<sub>3</sub>PO<sub>4</sub> photoanode, with enhanced light harvesting and crystal quality, exhibits 88% increase in (<em>J</em><sub>light</sub> − <em>J</em><sub>dark</sub>) value (1.94 mA cm<sup>−2</sup>) than non-annealed photoanode (1.03 mA cm<sup>−2</sup>). Moreover, it retains >99% current density after a 4000-s stability test. These results suggest that vacuum annealing can substantially improve the PEC performance of Ag<sub>3</sub>PO<sub>4</sub> microcrystalline film photoanodes due to mitigated effects of native defects, improved light harvesting, and inhibited Ag<sub>3</sub>PO<sub>4</sub> decomposition during water oxidation reaction.<span class="display"><span><ol class="links-for-figure"><li><a class="anchor download-link u-font-sans" href="https://ars.els-cdn.com/content/image/1-s2.0-S2352847821000678-ga1_lrg.jpg"><span class="anchor-text">Download : <span class="download-link-title">Download high-res image (141KB)</span></span></a></li><li><a class="anchor download-link u-font-sans" href="https://ars.els-cdn.com/content/image/1-s2.0-S2352847821000678-ga1.jpg"><span class="anchor-text">Download : <span class="download-link-title">Download full-size image</span></span></a></li></ol></span></span>
materials science, multidisciplinary,chemistry, physical,physics, applied