Raman Spectra, Infrared Spectra, and Microwave Dielectric Properties of Low‐Temperature Firing [(Li0.5Ln0.5)1−xCax]MoO4 (Ln = Sm and Nd) Solid Solution Ceramics with Scheelite Structure

haihong xi,di zhou,huidong xie,bin he,qiuping wang
DOI: https://doi.org/10.1111/jace.13332
IF: 4.186
2015-01-01
Journal of the American Ceramic Society
Abstract:In this work, a series of scheelite solid solution [(Li(0.5)Ln(0.5))(1-x)Ca-x]MoO4 (Ln=Sm and Nd; x=0.20, 0.40, 0.60, 0.70, 0.80, 0.85, 0.90) ceramics were prepared by conventional solid-state reaction method. The sintering temperature was lowered to 925 degrees C by (Li(0.5)Ln(0.5))(2+) substituting for Ca2+ in the solid solution without any secondary phase. Compared with that of scheelite CaMoO4 (-57ppm/degrees C), the temperature coefficient of resonant frequency (TCF or (f)) of the scheelite solid solution was modified to near zero (about +4.3ppm/degrees C) at x=0.8 with a dielectric constant 11.0 and the quality factor (Qxf value) of 18695GHz. The Raman spectra, showed the degree of disordering increased with x value, which resulted in decrease in the permittivities and increase in the Qxf values. The infrared spectra were analyzed using the classical harmonic oscillator model and were extrapolated to the microwave range. The chemical compatibility with silver electrode indicated that the reported series of ceramics were good candidates for the low-temperature cofired ceramic applications.
What problem does this paper attempt to address?