Phase evolution and microwave dielectric properties of (Li 0.5Bi0.5)(W1-xMox)O4 (0.0 ≤ x ≤ 1.0) ceramics with ultra-low sintering temperatures

Di Zhou,Jing Guo,Xi Yao,Lixia Pang,Zeming Qi,Tao Shao
DOI: https://doi.org/10.1142/S1793604712500427
IF: 1.4901
2012-01-01
Functional Materials Letters
Abstract:The (Li0.5Bi0.5)(W1-xMox)O-4 (0.0 <= x <= 1.0) ceramics were prepared via the solid state reaction method. The sintering temperature decreased almost linearly from 755 degrees C for (Li0.5Bi0.5)WO4 to 560 degrees C for (Li0.5Bi0.5)MoO4. When the x <= 0.3, a wolframite solid solution can be formed. For x = 0.4 and x = 0.6 compositions, both the wolframite and scheelite phases can be formed from the X-ray diffraction analysis, while two different kinds of grains can be revealed from the scanning electron microscopy and energy-dispersive X-ray spectrometer results. High performance of microwave dielectric properties were obtained in the (Li0.5Bi0.5)-(W0.6Mo0.4)O-4 ceramic sintered at 620 degrees C with a relative permittivity of 31.5, a Qf value of 8500 GHz (at 8.2 GHz), and a temperature coefficient value of +20ppm/degrees C. Complex dielectric spectra of pure (Li0.5Bi0.5)WO4 ceramic gained from the infrared spectra were extrapolated down to microwave range, and they were in good agreement with the measured values. The (Li0.5Bi0.5)-(W1-xMox)O-4 (0.0 <= x <= 1.0) ceramics might be promising for low temperature co-fired ceramic technology.
What problem does this paper attempt to address?