Microstructures and Electrochemical Properties of La0.7ce0.3ni3.7co0.7-Xal0.2mn0.4(Fe0.43b0.57)(X) (X=0-0.4) Hydrogen Storage Alloys

Zhou Yu,Fan Yanping,Peng Xianyun,Liu Baozhong
DOI: https://doi.org/10.4028/www.scientific.net/amr.608-609.917
2013-01-01
Abstract:X-ray diffraction results indicate that pristine alloy has a single LaNi5 phase and the alloys containing Fe0.43B0.57 consist of the matrix LaNi5 phase and the La3Ni13B2 secondary phase. The abundance of La3Ni13B2 phase increases with increasing x value. Maximum discharge capacity of the alloy electrodes monotonically decreases from 336.1 mAh/g (x = 0) to 281.2 mAh/g (x = 0.4). High-rate dischargeability of the alloy electrodes first increases with increasing x from 0 to 0.20, and then decreases when x increases to 0.4. Cycling stability decreases with increasing x from 0 to 0.4.