Effect of Co Content on the Structural and Electrochemical Properties of the La0.7Mg0.3Ni3.4−xMn0.1Cox Hydride Alloys
YF Liu,HG Pan,MX Gao,R Li,YQ Lei
DOI: https://doi.org/10.1016/j.jallcom.2004.01.010
IF: 6.2
2004-01-01
Journal of Alloys and Compounds
Abstract:In this paper, the structural, hydrogen storage and electrochemical studies were performed on the La0.7Mg0.3Ni3.4−xMn0.1Cox (x=0.00, 0.30, 0.60, 0.75, 0.90, 1.05, 1.15, 1.30, 1.45, 1.60) hydrogen storage alloys. The phase structures were identified by X-ray diffraction (XRD) and Rietveld analyses showing that all alloys consist mainly of two phases: the (La,Mg)Ni3 phase with the rhombohedral PuNi3-type structure and the LaNi5 phase with the hexagonal CaCu5-type structure besides a small amount of LaNi phase. Both a and c parameters of the (La,Mg)Ni3 phase and the LaNi5 phase increase with increasing Co content and a subsequent expansion of the cell volumes owing to the atomic radius of Co (1.67Å) being somewhat larger than that of Ni (1.62Å). Moreover, the abundances of the (La,Mg)Ni3 phase and the LaNi5 phase are changed relatively. P–C isotherms indicate that the equilibrium pressure for absorption/desorption hydrogen depresses steadily due to the expansion of the cell volume and the hydrogen storage capacity first increases and then decreases with increasing x from 0.00 to 1.60. Moreover, the absorption/desorption pressure hysteresis decreases and the plateau slope increases with the increase in Co content.