Preparation of Mnalc Flakes by Surfactant-Assisted Ball-Milling and the Effects of Annealing

K. P. Su,D. L. Tao,J. Wang,D. X. Huo,Y. Q. Cao,Z. W. Liu,Y. J. Zhang
DOI: https://doi.org/10.3139/146.111147
2015-01-01
International Journal of Materials Research
Abstract:An alternative approach for preparing anisotropic MnAlC powders is reported. [001] textured MnAlC flakes with various sizes and thicknesses were fabricated by surfactant-assisted ball-milling (SABM) of bulk ingots. After ball-milling for 8 h the flakes have thicknesses below 200 nm and aspect ratios as high as 102 similar to 10(3). After being annealed at suitable temperatures, both bulk and SABMed powders can transform from epsilon-phase to tau-phase completely. C-doping cannot prevent the decomposition of the tau-phase into the beta+gamma(2) phases after annealing at above 500 degrees C. The magnetic properties are strongly dependent on both the fraction of the tau-phase and the thickness. A high coercivity of similar to 242.8 kA m(-1) has been achieved in SABMed powders. The coercivity value is 128.8 % higher than the experimental value for bulk materials.
What problem does this paper attempt to address?