Effects of PbO-B 2 O 3 Glass Doping on the Sintering Temperature and Piezoelectric Properties of 0.35Pb (Ni 1/3 Nb 2/3 )O 3 -0.65Pb(Zr 0.41 Ti 0.59 )O 3 Ceramics

Jinqiao Yi,Meng Shen,Sisi Liu,Shenglin Jiang
DOI: https://doi.org/10.1007/s11664-015-4044-6
IF: 2.1
2015-01-01
Journal of Electronic Materials
Abstract:0.35Pb(Ni 1/3 Nb 2/3 )O 3 -0.65Pb(Zr 0.41 Ti 0.59 )O 3 (PNN-PZT) ceramics doped with 0.5PbO-0.5B 2 O 3 glass have been synthesized by the conventional solid-state sintering technique. The effects of 0.5PbO-0.5B 2 O 3 glass on the sintering temperature and piezoelectric properties of PNN-PZT ceramics were studied. The results indicated that the sintering temperature of PNN-PZT was significantly reduced due to the incorporation of 0.5PbO-0.5B 2 O 3 glass dopant. When the content of 0.5PbO-0.5B 2 O 3 glass was 0.5 wt.%, the sintering temperature of PNN-PZT was observed to reduce from above 1200°C to 920°C while the samples maintained high density (7.91 g/cm 3 ), excellent piezoelectric constant ( d 33 = 479 pC/N), large electromechanical coupling coefficient ( K p = 0.55), and relatively low electromechanical quality factor ( Q m = 79). Moreover, large dielectric constant ( ε 33 T / ε 0 = 2904) and low dielectric loss (tan δ = 0.0166) were obtained in this work.
What problem does this paper attempt to address?