Characterization of Fatigue Properties of Powder Metallurgy Titanium Alloy

Yuankui Cao,Fanpei Zeng,Bin Liu,Yong Liu,Jinzhong Lu,Ziyang Gan,Huiping Tang
DOI: https://doi.org/10.1016/j.msea.2015.12.058
2016-01-01
Abstract:The fatigue characteristics of powder metallurgy (P/M) Ti6Al4V (wt%) alloys prepared by powder sintering and hot rolling were studied under tension–tension loading conditions at R=0.1 and 25Hz in air, where R=σmin/σmax (σmin and σmax are the applied minimum and maximum stresses, respectively). The results show that for the as-sintered Ti6Al4V alloy the fatigue limit is about 325MPa, and the fatigue cracks initiate from the residual pores open to the surface of the gauge area and propagate along the α/β interfaces. Hot rolling markedly enhances the fatigue properties, and the fatigue limit increases to about 430MPa. The reducing of porosity and refining of grain size through hot rolling are the dominant mechanisms for the improvement of fatigue properties. In addition, the microstructure of α/β interfaces//RD and the texture of <0001>α//RD formed during hot rolling act as barriers for the fatigue crack propagation, which partly attributes to the improvement of the fatigue properties.
What problem does this paper attempt to address?