Vitrification of MSWI fly ash using direct current double arc plasma

王勤,严建华,潘新潮,池涌,高飞
DOI: https://doi.org/10.3785/j.issn.1008-973X.2011.01.024
2011-01-01
Abstract:The effects of additives SiO2 and CaO on heavy metal residual fraction and leaching toxicity were analyzed in order to evaluate the plasma treatment process and treatment effect of municipal solid waste incinerator (MSWI) fly ash vitrification. Fly ash samples with additives SiO2 and CaO were vitrified by thermal argon plasma arc at 1 400-1 500 °C. The chemical compositions, microstructures, crystalline phases and leaching toxicity of the fly ash and produced slag were determined by energy dispersion X-ray spectrometer analyzer (EDX), scanning electron microscopy (FSEM), X-ray diffractometry (XRD), and toxicity characteristic leaching procedure (TCLP), respectively. Results show that the slag is amorphous and plassy after thermal plasma vitrification. The mass concentration of heavy metal leaching from slags is much lower than the standards. Both the additions of SiO2 and CaO can keep heavy metals volatilizing from fly ash through vitrification, and CaO is more effective than SiO2 to prevent the volatilization of heavy metal. The additive SiO2 can reduce the leaching toxicity of slags, while CaO has opposite effects.
What problem does this paper attempt to address?