Process of indirect brazing alumina to 5A05 Al alloy

Fu-jia XU,Li-xia ZHANG,Ji-cai FENG,Ying WANG,Ke-qiang WANG
2010-01-01
Abstract:Vacuum brazing of Al alloy and electroless nickel plated alumina was carried out with Al-Si-Mg brazing alloy and Mg powder in home-made technical hood. Effects of brazing temperature and holding time on the interface structure and shear strength of joints were analyzed. The experimental results show that the interface structure is Al2O3/Ni(I zone)/Al3Ni2 (II zone)/Al3Ni+Mg2Si(III zone)/α(Al)+Mg2Si(IV zone)/5A05 when the brazing temperature is 570°C and holding time is 15 min. The maximum shear strength of joints is up to 25 MPa. As the holding time prolongs, Ni layer becomes thin, Al3Ni zone changes little and Al3Ni+Mg2Si zone becomes thick and dispersed. When the holding time is 50 min, Al3Ni+Mg2Si zone becomes scattered and Mg2Si near 5A05 alloy disappears. The effect of brazing temperature on the joints is similar to that of holding time. The fracture mode of joints is brittle. When the shear strength of joints is lower, the joints fracture near α(Al)+Mg2Si on Al alloy side. When the shear strength of joints is higher, the joints fracture on Ni+interface (II zone and III zone).
What problem does this paper attempt to address?