Abstract:High purity alumina ceramics were brazed to niobium metal to analyze the effects of brazing temperatures and Ti content in the active AgCuTi alloy filler on the joint microstructure,interfacial reactions and shear strengths. The results show that brazing temperatures of 825-900 ℃ do not significantly affect the joint strength,but that the joint strength decreases at temperatures higher than 900 ℃.The joint strength slightly decreases for Ti mass fractions of 1%-2%,while significantly decreasing for Ti mass fractions above 3%.The maximum joint shear strength reaches 100 MPa at 850 ℃ and a Ti mass fraction of 2% with a keeping time of 20 min.The interfacial reaction products adjacent to the alumina are mainly Cu3Ti3O and Ti oxide,in which the redundant Ti2O produced in the reaction layer at higher temperatures might be a key factor in reducing the joint strength.
What problem does this paper attempt to address?